UV-curable liquid silicone rubber / UV-PDMS

Unique Features

micro resist technology GmbH is providing a new selection of UV-curable liquid silicone rubber / UV-PDMS (OEM:Shin-Etsu) for European markets. The UV-PDMS can be used in a wide range of applications, but in particular for the manufacture of soft-molds in replication technologies such as nanoimprint lithography.

 

Application examples

Applications

There are two different types of UV-PDMS available. The following table provides the general material characteristics of the two different types of UV-PDMS:

General material characteristics of the new UV-PDMS (OEM:Shin-Etsu)

Main advantages by using the new Shin-Etsu UV-PDMS over generic PDMS:

  • Spin-coating for enhanced mold fabrication
  • Faster curing time (e.g. 10 min after UV exposure)
  • High resolution capabilities down 100 nm and smaller
  • 0.02% shrinkage for superb pattern fidelity
KER-4690 (X-34-4184) KER-4691 (X-34-4208)
Appearance (Color Tone) Colorless Milky-white
Appearance (Transparency) Transparent Semitransparent
Viscosity [Pa・s] 2.7 110
Hardness: Durometer type-A 55 42
Elongation at Break [%] 110 400
Tensile Strength [MPa] 7.7 7.0
Tear Propagation Strength (crescent)
[kN/m]
3.0 17.1
Linear Contraction [%] <0.1 <0.1
Curing Rate* [Min] 20 45
Curing Condition [mJ/cm2] 2000 2000

* TA Instruments ARES-G2, 25℃, 1Hz

Each system consists of two components. After thoroughly mixing the two-component material system (A/B) in equal volume, the liquid mixture compounds can be processed for up to 24 hours by casting, spin-coating or other deposition methods. Due to the photo-sensitivity, the cross-linking (or curing) is initiated by UV-exposure. In contrast to generic PDMS, this allows almost full curing already at room temperature and significantly increases the curing speed (by factor of 100 and more). Furthermore, without the need of an additional thermal curing one can achieve a minimized shrinkage of 0.02%.

 

For detailed information on material properties and process specifications, please get in contact with the unit manager NIL polymers Dr. Mirko Lohse (m.lohse@microresist.de). In case of inquiry request or purchase order, please contact our sales assistant Mrs. Anja Hinz (a.hinz@microresist.de).

quotation request

Assessment of Additive Manufacturing Processes for Monolithic Diffractive-Refractive Micro-Components
J Wolf et al., 2019 20th International Conference on Solid-State Sensors, Actuators and Microsystems & Eurosensors XXXIII (TRANSDUCERS & EUROSENSORS XXXIII)
Link: 10.1109/TRANSDUCERS.2019.8808288

Prototyping of Monolithic Diffractive-Refractive Micro-Optics with Inkjetable Polymers
J Wolf et al., Optical Design and Fabrication 2019 (Freeform, OFT)
Link: https://doi.org/10.1364/OFT.2019.OT2A.5

High fidelity 3D thermal nanoimprint with UV curable polydimethyl siloxane stamps
N Chidambaram et al., Journal of Vacuum Science & Technology B 34, 06K401 (2016)
Link: https://doi.org/10.1116/1.4961250

Contact us:

Anschrift
E-Mail(Required)
Drop files here or
Max. file size: 75 MB.
    Element 32
    0

    Resist Alliance

    micro resist technology is a single entry point for specialty chemicals used in micro and nano manufacturing in Europe. The portfolio of in-house products is complemented by the strategic sales of associated products that are manufactured by our international partners. Here we act as a high-service distributor and offer European medium-sized companies a wide range of complementary products from a single source, which can be used for both established and innovative production and manufacturing processes.

    Kayaku Advanced Materials, Inc. (formerly MicroChem Corp.)

    We offer photoresists and specialty chemicals for MEMS and microelectronic applications from our partner Kayaku Advanced Materials, with whom we have been working for more than 20 years.

    DJ MicroLaminates, Inc.

    We offer dry film resists for MEMS, microfluidics and packaging applications from our partner DJ MicroLaminates, with whom we have been cooperating for over two years.

    Dry Films

    Dry films are ready-to-use polymer films as laminate foil with a high accuracy of the film thickness and excellent adhesion behaviour on various substrates. They are very simple in handling, photo-structurable and both as cut sheets and as roll material available.

    • Available in different film thicknesses
    • UV-crosslinking as negative photoresist
    • Feasibility of high aspect ratios
    • Vertical sidewalls
    • Multi lamination possible – up to 6 layer  complex multi-layer designs
    • High chemical resilience

     

    • Application as permanent material for optical application (e.g. lenses, wave guides …), in micro fluidics

    Functional materials for inkjet-printing

    Special designed functional materials from the product groups Hybrid Polymers, Photoresists, and Nanoimprint Polymers for the deposition and alternative patterning using inkjet printing process

    • Available in different viscosities (adjustable)
    • Suitable in commercial inkjet printing devices
    • Focused on high reliability of droplet generation
    • UV-curable formulations

     

    • Usable as a permanent material for optical application (e.g. lenses, wave guides, optical couplers, diffractive elements, …)
    • Packaging material in the micro electronic
    • Deposition / patterning on substrates with surface topography
    • Imprint material for nano-structuring with high dose accuracy

    Nanoimprint Resists

    Nanoimprint Lithography (NIL) is a straight forward, low cost, and high throughput capable technology for the fabrication of nanometer scaled patterns. Main application fields are photonics, next generation electronics, as well as bio- and sensor applications.

    micro resist technology GmbH has provided tailor-made resist formulations for nanoimprint lithography (NIL) since 1999. The unique key features of our products are outstanding film forming and imprinting performance beside excellent pattern fidelity and plasma etch stability. Besides our highly innovative material developments in close contact to industrial needs, our strength is the ability to adjust our materials in film thickness as well as addressing certain needs of the specific use cases within the formulation. Our nanoimprint resists are mostly applied as an etch mask for pattern transfer into various substrates, like Si, SiO2, Al or sapphire.

    Our portfolio covers materials for the classical thermal NIL (T-NIL), in which a thermoplastic polymer is used, as well as UV-NIL, in which a liquid formulation is photo crosslinked upon photo exposure. With our technological expertise and know-how we are able to find the right material for your process and applications. Please contact us for your technical support!

    Hybrid Polymers

    micro resist technology offers a broad portfolio of UV-curable hybrid polymer products for micro-optical applications. Their excellent optical transparency and high thermal stability makes them perfectly suitable for the production of polymer-based optical components and waveguides. The main fields of application are micro lenses, diffractive optical elements (DOE), gratings, and single-mode or multi-mode waveguides.

    OrmoComp®: DE 30 210 075 433; IR 1 091 982 ; TW 100030626; OrmoClear®: DE 30 210 075 434; IR 1 091 359 ; TW 100030628; OrmoStamp®: DE 30 210 075 435; IR 1 092 621 ; TW 100030629; OrmoPrime®: DE 30 210 075 436

    Positive Photoresists

    Positive Photoresists for UV lithography (mask aligner, laser, greyscale exposure) and e-beam lithography

    • Variety of viscosities for 0.1 µm – 60 µm film thickness in one spin-coating step
    • Effective for broadband, g-line, h-line or i-line exposure, laser direct writing at 350…450 nm and e-beam lithography
    • No post exposure bake
    • Easy removal
       
    • For pattern transfer: Etch mask, mould for electroplating, mould for UV moulding
    • Use in microsystems technology, microelectronics, micro-optics – manufacture of e.g. MEMS, LEDs, ICs, MOEMS, fiber optics telecommunications devices, flat panel displays

    Negative Photoresists

    Photoresists for UV (mask aligner, laser)/ DUV and e-beam lithography

    • Effective for broadband and i-line, Deep UV, e-beam exposure, or laser direct writing @ 405 nm
    • Lift-off resists with tunable pattern profile, high temperature stability up to 160 °C
    • Variety of viscosities for different film thicknesses in one spin-coating step
       
    • For pattern transfer: Physical vapour deposition (PVD) and single  layer lift-off, etch mask, mould for electroplating
    • For permanent applications: Polymeric waveguides
    • Use in microsystems technology, microelectronics, micro-optics  – manufacture of e.g. LEDs, ICs, MEMS, flat panel displays, fiber optics telecommunications devices